VALIDATION OF AN OPTICAL SYSTEM TO MEASURE ACETABULAR SHELL DEFORMATION IN CADAVERS

The International Society for Technology in Arthroplasty (ISTA), 27th Annual Congress. PART 1.



Abstract

INTRODUCTION

Deformation of modular acetabular press-fit shells is a topic of much interest for surgeons and manufacturer. Such modular components utilise a titanium shell with a liner manufactured from metal, polyethylene or ceramic. Initial fixation is achieved through a press-fit between shell and acetabulum with the shell mechanically deforming upon insertion. Shell deformation may disrupt the assembly process of inserting the bearing liner into the acetabular shell for modular systems. This may adversely affect the integrity and durability of the components and the tribology of the bearing.

OBJECTIVE

Most clinically relevant data to quantify and understand such shell deformation can be achieved by cadaver measurements. ATOS Triple Scan III was identified as a measurement system with the potential to perform those measurements. The study aim was to validate an ATOS Triple Scan III optical measurement system against a co-ordinate measuring machine (CMM) using in-vitro testing and to check capability/ repeatability under cadaver lab conditions.

METHODS

Two sizes of custom-made acetabular shells were deformed using a uniaxial/ two-point loading frame and measured repeatedly at different loads. Roundness measurements were performed using both the ATOS Triple Scan III optical system and a co-ordinate measuring machine and then compared. The repeatability was also tested by measuring shells pre and post insertion in a cadaver lab multiple times.

RESULTS

The in-vitro comparison with CMM demonstrated a maximum difference of 5 µm at the rim and 9 µm at the measurement point closest to the pole of the shell. Deviation between the two systems increased towards the pole for the in-vitro measurements. However as press fit shells are designed to be loaded at the rim, this is likely where the maximum deflection will occur as a result of the highest force. Therefore, the increased difference between the systems towards the pole is of less importance compared with accuracy at the rim. Maximum repeatability was below 1 µm for the CMM and 3 µm for the ATOS Triple Scan III optical system. Repeatability of the ATOS Triple Scan III optical system was comparable between pre insertion (below 2 µm) and post insertion (below 3 µm) measurements in the cadaver lab. In addition these values were comparable to the repeatability measured during the in-vitro validation study (below 3 µm). This proves high repeatability not only for in-vitro conditions, but also for the cadaver lab as well.

CONCLUSIONS

This study supports the view that the ATOS Triple Scan III optical system fulfils the necessary requirements to accurately measure shell deformation in cadavers. As a result, the authors propose further studies using cadavers to identify the impact of other factors upon shell deformation. Other factors to be measured include bone strength, shell diameter, under reaming and wall thickness.